Phone:
0086-0731-88678530
Email:
sales@bestar-pipe.com
English
Home
Products
Carbon Steel Pipe
Carbon Steel Seamless Pipe
Carbon Steel Welded Pipe
OCTG Casing and Tubing Pipe
Stainless Steel Pipe
304 Pipe
316 Pipe
Stainless Steel Seamless Pipe
Stainless Steel Welded Pipe
Duplex Steel Seamless Pipe
Duplex Steel Welded Pipe
Alloy Steel Pipe
Alloy Steel Seamless Pipe
Alloy Steel Welded Pipe
Pipe Fittings
Carbon Steel Fittings
Stainless Steel Fittings
Alloy Steel Fittings
Flange
Flange
Steel Plate / Coil
Carbon Steel Plate
Stainless Steel Plate
Carbon Steel Coil
Stainless Steel Coil
Project
Quality Control
About Us
History
Factory Tour
Certificate
News
Contact Us
Download
Project
Oil & Gas Transmission
by admin on 22-02-10
24″ & 12″ Pipeline & Pump Station Project Project introduction: 3 Km Pipeline & 2500 Dia inch Piping, ROW, Stringing, Bending, Welding, Blasting & Coating & Painting, Fabrication, Steel Supports, Trenching, Beddi...
Read more
Marine & Offshore
by admin on 22-02-10
Odyssea Marine Project in Mexico Project introduction: operate a worldwide capable fleet of Dynamic Positioning 2 and Dynamic Positioning 1 offshore vessels ranging from 265' in length to 170' in length. The shipyard also ha...
Read more
Exploration & Drilling Services
by admin on 22-02-10
Anis Marinetime Project in Italy Project introduction: in shipbuilding and ship repair markets, continuous search and development, mastering new technologies, highlyskilled workers, engineers and managers. Location:...
Read more
Construction
by admin on 22-02-08
Infrastructure project construction in Jordan Project introduction: According to project needs, provide durable industrial pipes and steel product solutions for this construction project, including underground pipes, drainag...
Read more
<<
< Previous
1
2
Want To Cooperate With Us?
Contact us today for consultation.
Welcome inquiry
Reply to you as soon as possible
English
French
German
Portuguese
Spanish
Russian
Japanese
Korean
Arabic
Turkish
Italian
Indonesian
Filipino
Malay
Thai
Vietnamese