1. Spiral steel pipes must not be stacked together with acid, alkali, salt, cement, and other materials that are corrosive to steel in the warehouse. Different types of steel should be stacked separately to prevent confusion and contact corrosion;
2. Large steel sections, rails, steel plates, large-diameter spiral steel pipes, forgings, etc. can be stacked in the open air;
3. Small and medium-sized steel, wire rods, steel bars, medium-diameter steel pipes, steel wires, and steel wire ropes, etc., can be stored in well-ventilated sheds, but they must be covered with thatch;
4. Spiral steel pipe warehouses should be selected based on geographical conditions. Generally, ordinarily, closed warehouses are used, that is, warehouses with walls on the roof, tight doors and windows, and ventilation devices;
5. Some small steel products, thin steel plates, steel strips, silicon steel sheets, small diameter or thin-walled steel pipes, various cold-rolled and cold-drawn steel products, and high-priced and corrosive metal products can be stored in the warehouse;
6. The site or warehouse where spiral steel pipe products are kept should be selected in a clean place with smooth drainage and away from factories and mines that produce harmful gases or dust. Weeds and all debris should be removed from the site and the steel should be kept clean;
7. The warehouse is required to be well-ventilated on sunny days, closed to prevent moisture on rainy days, and should always be properly stored.