Characteristics of epoxy resin anti-corrosion steel pipe: good durability, the paint film after epoxy resin curing is tough and water-resistant, and the coating film is non-toxic and does not pollute water. Strong adhesion, the paint film has good adhesion. Excellent anti-rust and water resistance, the use of excellent anti-rust raw materials can ensure its anti-rust performance. It has good mechanical strength, tough paint film, wear resistance, and impact resistance. High solid content, thick coating film. Curing film at room temperature. No large baking equipment is required.
Application fields of epoxy resin anti-corrosion steel pipe: widely used in the inner wall coating of water supply equipment such as drinking water tanks, water pipes, water tanks, water towers, and sugar and grain cargo holds. It can also be used as the inner wall coating of swimming pools, power plant cooling towers, and metal and concrete for fuel oil and gasoline.
Construction and storage of epoxy resin anti-corrosion steel pipes
(1) Before painting, the dust, oil, scale, etc. on the surface of the object must be cleaned. Reach Sa 2.5 level to ensure the quality of the painting. It is strictly forbidden to bring in moisture during construction.
(2) The construction ratio method is: open the mouth of component A, add component B into component A, and stir thoroughly. After aging for 30 minutes, you can start painting.
(3) This material requires use as soon as it is mixed. The paint after mixing must be used up within eight hours. Unmixed materials must be sealed and stored. Construction should be stopped on rainy days or when the relative temperature is greater than 75%. For areas with severe corrosive media, it is recommended to apply multiple coats.
(4) The product should be stored in a cool and dry place, avoid direct sunlight, be isolated from fire sources, and stay away from heat sources. The storage period is twelve months. After the expiration of the period, various technical indicators should be tested. If the indicator requirements are met, it can continue to be used.
Post time: Nov-01-2024