Alloy Steel Pipe

  • Alloy Steel Seamless Pipe

    Alloy Steel Seamless Pipe

    Type: Alloy Tube, Alloy Steel Tube, Seamless Alloy Steel Tube
    Spec.: OD: 1/8” ~ 26”. WT: SCH 30, 30, 40, 60, 80, 120, 140, 160, XS, XXS, STD. LENGTH: Single, Double Random, etc.
    Standard & Grade: GB/T 3091 , BS1387, EN39, EN1139, ASTM A53, A335, JIS G3444
    Grade: Q195, Q215, Q235, Q345, S235JR, S275JR, STK 400, STK 500

    Ends: Plain End, Beveled End, Thread End
    Coating: Zinc coating: 10~50 g/m2

  • Alloy Steel Welded Pipe

    Alloy Steel Welded Pipe

    Type: Alloy Pipe, Alloy Tube, Alloy Steel Pipe, Alloy Steel Tube, Alloy Welded Steel Pipe
    Spec.: OD: Norminal~60”. WT: up through 4”. Length: Single Random, Double Random, Cut length max to 23m.
    Standard: ASTM A691 (Rolled & Welded)
    Grade: 1-1/4 CR, 2-1 1/4 CR, 5 CR, 9 CR 91
    End: Plain End, Beveled End, Thread End
    Packing: Bundled with Hemp Rope/In Bulk
    Application: In Petroleum, Aerospace, Chemical, Power, Boiler, Military Industry